PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Volume Resistivity | 1.E+02 - 1.E+06 | Ω.cm | ASTM D257 |
Surface Resistivity | 1.E+02 - 1.E+06 | Ω | ASTM D257 |
LNP STAT-KON EE003XXC compound is based on Polyetherimide (PEI) resin containing 15% carbon fiber. Added features of this grade include: LNP Clean Compounding Technology, Electrically Conductive.
All colors are customizable. Refer our ColorXpress tool to check color availability
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Volume Resistivity | 1.E+02 - 1.E+06 | Ω.cm | ASTM D257 |
Surface Resistivity | 1.E+02 - 1.E+06 | Ω | ASTM D257 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Izod Impact, unnotched, 23°C | 373 | J/m | ASTM D4812 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Extended Drying Temperature | 150 | °C | |
Drying Time | 4 - 6 | Hrs | |
Maximum Moisture Content | 0.02 | % | |
Melt Temperature | 360 - 400 | °C | |
Rear - Zone 1 Temperature | 360 - 380 | °C | |
Middle - Zone 2 Temperature | 370 - 390 | °C | |
Front - Zone 3 Temperature | 380 - 400 | °C | |
Nozzle Temperature | 390 - 400 | °C | |
Mold Temperature | 140 - 180 | °C | |
Back Pressure | 0.3 - 0.7 | MPa | |
Screw speed (Circumferential speed) | 0.2 - 0.3 | m/s | |
Vent Depth | 0.025 - 0.076 | mm |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Tensile Stress, break | 165 | MPa | ASTM D638 |
Tensile Strain, break | 1.6 | % | ASTM D638 |
Flexural Stress | 248 | MPa | ASTM D790 |
Flexural Modulus | 11720 | MPa | ASTM D790 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Density | 1.33 | g/cm³ | ASTM D792 |
Mold Shrinkage, flow, 24 hrs | 0.1 - 0.3 | % | ASTM D955 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Relative Temp Index, Elec | 105 | °C | UL 746B |
Relative Temp Index, Mech w/impact | 105 | °C | UL 746B |
Relative Temp Index, Mech w/o impact | 105 | °C | UL 746B |