IMPACT
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Izod Impact, unnotched, 23°C | 1238 | J/m | ASTM D4812 |
Izod Impact, notched, 23°C | 352 | J/m | ASTM D256 |
LNP THERMOCOMP 2C003 compound is based on Ethylene Tetrafluoroethylene (ETFE) resin containing 15% carbon fiber. Added features of this grade include: Electrically Conductive.
All colors are customizable. Refer our ColorXpress tool to check color availability
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Izod Impact, unnotched, 23°C | 1238 | J/m | ASTM D4812 |
Izod Impact, notched, 23°C | 352 | J/m | ASTM D256 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Drying Temperature | 120 - 150 | °C | |
Drying Time | 4 | Hrs | |
Melt Temperature | 315 | °C | |
Front - Zone 3 Temperature | 325 - 340 | °C | |
Middle - Zone 2 Temperature | 300 - 325 | °C | |
Rear - Zone 1 Temperature | 280 - 300 | °C | |
Mold Temperature | 90 - 120 | °C | |
Back Pressure | 0.2 - 0.3 | MPa | |
Screw Speed | 30 - 60 | rpm |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Tensile Stress, break | 90 | MPa | ASTM D638 |
Tensile Stress, brk, Type I, 5 mm/min | 90 | MPa | ASTM D638 |
Tensile Strain, break | 4.9 | % | ASTM D638 |
Tensile Strain, brk, Type I, 5 mm/min | 4.9 | % | ASTM D638 |
Tensile Modulus, 50 mm/min | 11710 | MPa | ASTM D638 |
Flexural Stress | 137 | MPa | ASTM D790 |
Flexural Stress, brk, 1.3 mm/min, 50 mm span | 137 | MPa | ASTM D790 |
Flexural Modulus | 11030 | MPa | ASTM D790 |
Flexural Modulus, 1.3 mm/min, 50 mm span | 11030 | MPa | ASTM D790 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Density | 1.73 | g/cm³ | ASTM D792 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
HDT, 1.82 MPa, 3.2mm, unannealed | 207 | °C | ASTM D648 |