FLAME CHARACTERISTICS
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
UL Yellow Card Link | View | - | - |
UL Recognized, 94V-0 Flame Class Rating | 2.5 | mm | UL 94 |
UL Recognized, 94V-1 Flame Class Rating | ≥1.5 | mm | UL 94 |
NORYL FP3060 resin is a non-reinforced blend of polyphenylene ether (PPE) + polystyrene (PS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant with a UL94 flame rating of V0 at 2.5mm and V0 at 2.5mm. NORYL FP3060 resin was designed to have very good dimensional stability with high flow and exhibits good rheological properties, high heat resistance, hydrolysis resistance, and very low density. The combination of these properties makes this material an excellent candidate for Flat Panel TV enclosure applications.
All colors are customizable. Refer our ColorXpress tool to check color availability
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
UL Yellow Card Link | View | - | - |
UL Recognized, 94V-0 Flame Class Rating | 2.5 | mm | UL 94 |
UL Recognized, 94V-1 Flame Class Rating | ≥1.5 | mm | UL 94 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Izod Impact, notched, 23°C | 78 | J/m | ASTM D256 |
Izod Impact, notched 80*10*4 +23°C | 6 | kJ/m² | ISO 180/1A |
Izod Impact, notched 80*10*4 -30°C | 5 | kJ/m² | ISO 180/1A |
Charpy 23°C, V-notch Edgew 80*10*4 sp=62mm | 6 | kJ/m² | ISO 179/1eA |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Drying Temperature | 65 - 75 | °C | |
Drying Time | 2 - 3 | Hrs | |
Melt Temperature | 250 - 285 | °C | |
Nozzle Temperature | 240 - 270 | °C | |
Front - Zone 3 Temperature | 250 - 285 | °C | |
Middle - Zone 2 Temperature | 230 - 260 | °C | |
Rear - Zone 1 Temperature | 200 - 220 | °C | |
Hopper Temperature | 60 - 80 | °C | |
Mold Temperature | 40 - 65 | °C |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Tensile Stress, yld, Type I, 50 mm/min | 54 | MPa | ASTM D638 |
Tensile Stress, brk, Type I, 50 mm/min | 55 | MPa | ASTM D638 |
Tensile Strain, yld, Type I, 50 mm/min | 3 | % | ASTM D638 |
Tensile Strain, brk, Type I, 50 mm/min | 12 | % | ASTM D638 |
Tensile Modulus, 50 mm/min | 2200 | MPa | ASTM D638 |
Flexural Stress, yld, 1.3 mm/min, 50 mm span | 84 | MPa | ASTM D790 |
Flexural Modulus, 1.3 mm/min, 50 mm span | 2400 | MPa | ASTM D790 |
Tensile Stress, yield, 50 mm/min | 55 | MPa | ISO 527 |
Tensile Stress, break, 50 mm/min | 42 | MPa | ISO 527 |
Tensile Strain, yield, 50 mm/min | 3 | % | ISO 527 |
Tensile Strain, break, 50 mm/min | 11 | % | ISO 527 |
Tensile Modulus, 1 mm/min | 2420 | MPa | ISO 527 |
Flexural Stress, yield, 2 mm/min | 82 | MPa | ISO 178 |
Flexural Modulus, 2 mm/min | 2530 | MPa | ISO 178 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Specific Gravity | 1.1 | - | ASTM D792 |
Density | 1.1 | g/cm³ | ISO 1183 |
Water Absorption, (23°C/saturated) | 0.13 | % | ISO 62-1 |
Moisture Absorption (23°C / 50% RH) | 0.02 | % | ISO 62 |
Melt Volume Rate, MVR at 280°C/1.2 kg | 20 | cm³/10 min | ISO 1133 |
Melt Volume Rate, MVR at 280°C/2.16 kg | 41 | cm³/10 min | ISO 1133 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Vicat Softening Temp, Rate B/50 | 105 | °C | ASTM D1525 |
HDT, 1.82 MPa, 3.2mm, unannealed | 80 | °C | ASTM D648 |
CTE, -40°C to 40°C, flow | 8.3E-05 | 1/°C | ASTM E831 |
CTE, -40°C to 40°C, xflow | 8.E-05 | 1/°C | ASTM E831 |
CTE, -40°C to 40°C, flow | 8.3E-05 | 1/°C | ISO 11359-2 |
CTE, -40°C to 40°C, xflow | 8.E-05 | 1/°C | ISO 11359-2 |
Vicat Softening Temp, Rate B/50 | 91 | °C | ISO 306 |
Vicat Softening Temp, Rate B/120 | 93 | °C | ISO 306 |
HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm | 74 | °C | ISO 75/Af |
Relative Temp Index, Elec | 65 | °C | UL 746B |
Relative Temp Index, Mech w/impact | 65 | °C | UL 746B |
Relative Temp Index, Mech w/o impact | 65 | °C | UL 746B |