ELECTRICAL
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Surface Resistivity | 1.E+16 | Ω | ASTM D257 |
Relative Permittivity, 50/60 Hz | 2.78 | - | ASTM D150 |
Dissipation Factor, 50/60 Hz | 0.003 | - | ASTM D150 |
NORYL N1050 resin is a non-reinforced blend of polyphenylene ether (PPE) + polystyrene (PS). This injection moldable grade was designed for improved dimensional stability and flow. This grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm and V0 at 1.5mm along with impact strength, very low moisture absorption, excellent dimensional stability, and good electrical properties. NORYL N1050 resin is an excellent candidate for a variety of applications requiring electrically insulating properties, low moisture absorption and low warpage.
All colors are customizable. Refer our ColorXpress tool to check color availability
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Surface Resistivity | 1.E+16 | Ω | ASTM D257 |
Relative Permittivity, 50/60 Hz | 2.78 | - | ASTM D150 |
Dissipation Factor, 50/60 Hz | 0.003 | - | ASTM D150 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
UL Recognized, 94V-0 Flame Class Rating | 1.5 | mm | UL 94 |
UL Recognized, 94-5VA Flame Class Rating | 2.5 | mm | UL 94 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Izod Impact, notched, 23°C | 117 | J/m | ASTM D256 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Drying Temperature | 75 - 80 | °C | |
Drying Time | 3 - 4 | Hrs | |
Drying Time (Cumulative) | 8 | Hrs | |
Maximum Moisture Content | 0.02 | % | |
Melt Temperature | 250 - 275 | °C | |
Nozzle Temperature | 250 - 275 | °C | |
Front - Zone 3 Temperature | 240 - 275 | °C | |
Middle - Zone 2 Temperature | 225 - 270 | °C | |
Rear - Zone 1 Temperature | 215 - 265 | °C | |
Mold Temperature | 55 - 75 | °C | |
Back Pressure | 0.3 - 0.7 | MPa | |
Screw Speed | 20 - 100 | rpm | |
Shot to Cylinder Size | 30 - 70 | % | |
Vent Depth | 0.038 - 0.051 | mm |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Tensile Stress, yield | 63 | MPa | SABIC - Japan Method |
Tensile Strain, break | 40 | % | SABIC - Japan Method |
Flexural Stress | 98 | MPa | ASTM D790 |
Flexural Modulus | 2530 | MPa | ASTM D790 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Specific Gravity | 1.1 | - | ASTM D792 |
Water Absorption, (23°C/24hrs) | 0.07 | % | ASTM D570 |
Mold Shrinkage, flow, 3.2 mm | 0.5 - 0.7 | % | SABIC method |
Melt Flow Rate, 250°C/10.0 kgf | 17 | g/10 min | ASTM D1238 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
HDT, 1.82 MPa, 6.4 mm, unannealed | 105 | °C | ASTM D648 |
CTE, -30°C to 30°C | 7.00E-05 | 1/°C | TMA |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Surface Resistivity | 1.E+16 | Ω | ASTM D257 |
Relative Permittivity, 50/60 Hz | 2.78 | - | ASTM D150 |
Dissipation Factor, 50/60 Hz | 0.003 | - | ASTM D150 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
UL Recognized, 94V-0 Flame Class Rating | 1.5 | mm | UL 94 |
UL Recognized, 94-5VA Flame Class Rating | 2.5 | mm | UL 94 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Izod Impact, notched, 23°C | 117 | J/m | ASTM D256 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Drying Temperature | 75 - 80 | °C | |
Drying Time | 3 - 4 | Hrs | |
Drying Time (Cumulative) | 8 | Hrs | |
Maximum Moisture Content | 0.02 | % | |
Melt Temperature | 250 - 275 | °C | |
Nozzle Temperature | 250 - 275 | °C | |
Front - Zone 3 Temperature | 240 - 275 | °C | |
Middle - Zone 2 Temperature | 225 - 270 | °C | |
Rear - Zone 1 Temperature | 215 - 265 | °C | |
Mold Temperature | 55 - 75 | °C | |
Back Pressure | 0.3 - 0.7 | MPa | |
Screw Speed | 20 - 100 | rpm | |
Shot to Cylinder Size | 30 - 70 | % | |
Vent Depth | 0.038 - 0.051 | mm |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Tensile Stress, yield | 63 | MPa | SABIC - Japan Method |
Tensile Strain, break | 40 | % | SABIC - Japan Method |
Flexural Stress | 98 | MPa | ASTM D790 |
Flexural Modulus | 2530 | MPa | ASTM D790 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Specific Gravity | 1.1 | - | ASTM D792 |
Water Absorption, (23°C/24hrs) | 0.07 | % | ASTM D570 |
Mold Shrinkage, flow, 3.2 mm | 0.5 - 0.7 | % | SABIC method |
Melt Flow Rate, 250°C/10.0 kgf | 17 | g/10 min | ASTM D1238 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
HDT, 1.82 MPa, 6.4 mm, unannealed | 105 | °C | ASTM D648 |
CTE, -30°C to 30°C | 7.00E-05 | 1/°C | TMA |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Surface Resistivity | 1.E+16 | Ω | ASTM D257 |
Relative Permittivity, 50/60 Hz | 2.78 | - | ASTM D150 |
Dissipation Factor, 50/60 Hz | 0.003 | - | ASTM D150 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
UL Recognized, 94V-0 Flame Class Rating | 1.5 | mm | UL 94 |
UL Recognized, 94-5VA Flame Class Rating | 2.5 | mm | UL 94 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Izod Impact, notched, 23°C | 117 | J/m | ASTM D256 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Drying Temperature | 75 - 80 | °C | |
Drying Time | 3 - 4 | Hrs | |
Drying Time (Cumulative) | 8 | Hrs | |
Maximum Moisture Content | 0.02 | % | |
Melt Temperature | 250 - 275 | °C | |
Nozzle Temperature | 250 - 275 | °C | |
Front - Zone 3 Temperature | 240 - 275 | °C | |
Middle - Zone 2 Temperature | 225 - 270 | °C | |
Rear - Zone 1 Temperature | 215 - 265 | °C | |
Mold Temperature | 55 - 75 | °C | |
Back Pressure | 0.3 - 0.7 | MPa | |
Screw Speed | 20 - 100 | rpm | |
Shot to Cylinder Size | 30 - 70 | % | |
Vent Depth | 0.038 - 0.051 | mm |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Tensile Stress, yield | 63 | MPa | SABIC - Japan Method |
Tensile Strain, break | 40 | % | SABIC - Japan Method |
Flexural Stress | 98 | MPa | ASTM D790 |
Flexural Modulus | 2530 | MPa | ASTM D790 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
Specific Gravity | 1.1 | - | ASTM D792 |
Water Absorption, (23°C/24hrs) | 0.07 | % | ASTM D570 |
Mold Shrinkage, flow, 3.2 mm | 0.5 - 0.7 | % | SABIC method |
Melt Flow Rate, 250°C/10.0 kgf | 17 | g/10 min | ASTM D1238 |
PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
---|---|---|---|
HDT, 1.82 MPa, 6.4 mm, unannealed | 105 | °C | ASTM D648 |
CTE, -30°C to 30°C | 7.00E-05 | 1/°C | TMA |
view multipoint data represented visually on graphs.
You may click on the curve legends to select/unselect the curves.
Please login to view graphs, download multi-point data or literature
Please login to view graphs, download multi-point data or literature
Your PDF is downloading. Please wait.