FLAME CHARACTERISTICS
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| UL Yellow Card Link | View | - | - |
| UL Recognized, 94V-2 Flame Class Rating | ≥0.8 | mm | UL 94 |
NORYL N802 resin is a non-reinforced blend of polyphenylene ether (PPE) + polystyrene (PS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V2 at 0.8mm. NORYL N802 resin exhibits high flow, good dimensional stability, and low specific gravity. It is an excellent candidate for a variety of printer applications.
All colors are customizable. Refer our ColorXpress tool to check color availability
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| UL Yellow Card Link | View | - | - |
| UL Recognized, 94V-2 Flame Class Rating | ≥0.8 | mm | UL 94 |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| Izod Impact, notched, 23°C | 78 | J/m | ASTM D256 |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| Drying Temperature | 80 - 85 | °C | |
| Drying Time | 2 - 4 | Hrs | |
| Drying Time (Cumulative) | 8 | Hrs | |
| Melt Temperature | 230 | °C | |
| Nozzle Temperature | 190 - 230 | °C | |
| Front - Zone 3 Temperature | 190 - 230 | °C | |
| Middle - Zone 2 Temperature | 190 - 230 | °C | |
| Rear - Zone 1 Temperature | 175 - 225 | °C | |
| Mold Temperature | 40 - 65 | °C | |
| Back Pressure | 0.3 - 0.7 | MPa | |
| Screw Speed | 20 - 100 | rpm | |
| Shot to Cylinder Size | 30 - 70 | % | |
| Vent Depth | 0.038 - 0.051 | mm |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| Tensile Stress, yield | 35 | MPa | SABIC - Japan Method |
| Tensile Strain, break | 50 | % | SABIC - Japan Method |
| Flexural Stress | 53 | MPa | ASTM D790 |
| Flexural Modulus | 2150 | MPa | ASTM D790 |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| Specific Gravity | 1.08 | - | ASTM D792 |
| Water Absorption, (23°C/24hrs) | 0.07 | % | ASTM D570 |
| Mold Shrinkage, flow, 3.2 mm | 0.5 - 0.7 | % | SABIC method |
| Melt Flow Rate, 260°C/2.16 kgf | 21 | g/10 min | ASTM D1238 |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| HDT, 1.82 MPa, 6.4 mm, unannealed | 80 | °C | ASTM D648 |
| CTE, -30°C to 30°C | 7.00E-05 | 1/°C | TMA |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| UL Yellow Card Link | View | - | - |
| UL Recognized, 94V-2 Flame Class Rating | ≥0.8 | mm | UL 94 |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| Izod Impact, notched, 23°C | 78 | J/m | ASTM D256 |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| Tensile Stress, yield | 35 | MPa | SABIC - Japan Method |
| Tensile Strain, break | 50 | % | SABIC - Japan Method |
| Flexural Stress | 53 | MPa | ASTM D790 |
| Flexural Modulus | 2150 | MPa | ASTM D790 |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| Specific Gravity | 1.08 | - | ASTM D792 |
| Water Absorption, (23°C/24hrs) | 0.07 | % | ASTM D570 |
| Mold Shrinkage, flow, 3.2 mm | 0.5 - 0.7 | % | SABIC method |
| Melt Flow Rate, 260°C/2.16 kgf | 21 | g/10 min | ASTM D1238 |
| PROPERTIES | TYPICAL VALUES | UNITS | TEST METHODS |
|---|---|---|---|
| HDT, 1.82 MPa, 6.4 mm, unannealed | 80 | °C | ASTM D648 |
| CTE, -30°C to 30°C | 7.00E-05 | 1/°C | TMA |